Method for producing a molded part made of plastic and provided with a UV-cured paint, and said molded part
First Claim
1. A process for production, in an injection mold, of a plastics molding with a UV-cured lacquer and with a visible area designed as functional area, where the UV-cured lacquer forms said visible area, comprisingarranging a film segment that has not been preformed and that is in essence flat, composed of a carrier layer made of a thermoplastic and of a partially thermally cured UV-curable lacquer in a cavity of the injection mold in such a way that the partially cured lacquer layer faces toward a female-mold surface replicating the negative form of the visible area of the molding, andsubjecting the film segment arranged in the cavity to insert molding with a thermoplastic on a reverse-side surface facing away from the partially thermally cured UV-curable lacquer, in such a way that the carrier layer of the film segment bonds to the injected hot melt, andwherein a compressive force resulting from the injection pressure of the injected melt acts in the direction of the female-mold surface, whereupon, with exposure to the compressive force and to heating resulting from the direct contact with the hot melt, the entire area of the film segment is forced onto the female-mold surface and subjected to a three-dimensional forming process,removing of the molding, and curing the partially thermally cured UV-curable lacquer to completion by UV radiation and, on the molding, forming the visible area designed as functional area.
2 Assignments
0 Petitions
Accused Products
Abstract
The invention relates to as method for producing a molded part in an injection mold, which molded part is made of plastic and provided with a UV-cured paint, wherein the UV-cured paint forms a visible surface designed as a functional surface. The invention further relates to such a molded part provided with a UV-cured paint, said molded part having a visible surface designed as a functional surface, wherein the UV-cured paint forms said visible surface.
14 Citations
7 Claims
-
1. A process for production, in an injection mold, of a plastics molding with a UV-cured lacquer and with a visible area designed as functional area, where the UV-cured lacquer forms said visible area, comprising
arranging a film segment that has not been preformed and that is in essence flat, composed of a carrier layer made of a thermoplastic and of a partially thermally cured UV-curable lacquer in a cavity of the injection mold in such a way that the partially cured lacquer layer faces toward a female-mold surface replicating the negative form of the visible area of the molding, and subjecting the film segment arranged in the cavity to insert molding with a thermoplastic on a reverse-side surface facing away from the partially thermally cured UV-curable lacquer, in such a way that the carrier layer of the film segment bonds to the injected hot melt, and wherein a compressive force resulting from the injection pressure of the injected melt acts in the direction of the female-mold surface, whereupon, with exposure to the compressive force and to heating resulting from the direct contact with the hot melt, the entire area of the film segment is forced onto the female-mold surface and subjected to a three-dimensional forming process, removing of the molding, and curing the partially thermally cured UV-curable lacquer to completion by UV radiation and, on the molding, forming the visible area designed as functional area.
-
2. The process as claimed in claim 1, wherein, before and/or during and/or after the production of the molding, at least a region delimiting the cavity within the injection mold is subjected to temperature control.
-
3. The process as claimed in claim 1, wherein, in the region of an injection aperture of the injection mold, the film segment is fixed in such a way that the compressive force resulting from the injection pressure of the injected melt acts toward a reverse-side surface facing away from the lacquer layer on the film segment.
-
4. The process as claimed in claim 1, wherein the thermoplastic injected is loaded with a blowing agent.
-
5. The process as claimed claim 1, wherein, before the film segment is subjected to insert molding, a color is applied at least on a section of a reverse-side surface facing away from the lacquer layer of the film segment.
-
6. The process as claimed in claim 1, wherein at least one functional element is injection-molded onto the molding.
-
7. The process as claimed in claim 1, wherein the molding is produced by subjecting the film segment to insert molding in the single- or multicomponent injection-molding process.
Specification