ADDITIVE FOR RECLAMATION OF ASPHALT, RECLAIMED ASPHALT PAVEMENT MATERIAL CONTAINING SAME, MODIFIED ASPHALT, AND ASPHALT PAVEMENT MATERIAL CONTAINING SAME
2 Assignments
0 Petitions
Accused Products
Abstract
An additive for reclaiming asphalt of the present invention, which is obtained by adding straight asphalt to a mixture of a waste animal or vegetable oil and a waste mineral oil having a kinematic viscosity at 60° C. of 10 mm2/s to 40 mm2/s, mixing the materials, and heating the resultant mixture to remove an aromatic component. The additive for reclaiming asphalt can restore the physical properties of a deteriorated asphalt component to the same or greater extent than that of a conventional additive for reclaiming asphalt, and the additive has low content of components that may affect the environment or humans, and high fluidity at room temperature, and is available at an extremely low cost.
5 Citations
14 Claims
-
1-5. -5. (canceled)
-
6. A method of producing an additive for reclaiming asphalt, comprising:
-
adding straight asphalt to a mixture of (a) waste animal and/or vegetable oil and (b) a waste mineral oil having a kinematic viscosity at 60°
C. of 10 mm2/s to 40 mm2/s,mixing the materials, heating the resultant mixture thereby removing an aromatic component, and obtaining the additive for reclaiming asphalt. - View Dependent Claims (7, 8, 9, 10, 11, 12)
-
-
13. A method of producing a modified asphalt, comprising adding a xerogel-like amorphous resin to molten straight asphalt together with a waste animal or vegetable oil and mixing the materials,
wherein the xerogel-like amorphous resin is obtained by dissolving an amorphous resin with an organic solvent capable of dissolving the amorphous resin to provide a gel- or dough-like amorphous resin in a saturated state, immersing the resin in alcohol to remove the organic solvent, and drying the remainder.
-
14. A method of producing a modified asphalt, comprising adding a product to molten straight asphalt together with a waste animal or vegetable oil and mixing the materials,
wherein the product is obtained by dissolving an amorphous resin with an organic solvent capable of dissolving the amorphous resin to provide a gel- or dough-like amorphous resin in a saturated state, and heating the resin to melt the resin, and wherein a content of the gel- or dough-like amorphous resin in the modified asphalt is 70 wt % to 90 wt %.
Specification