MAGNETIC RECORDING MEDIUM
First Claim
1. A magnetic recording medium comprising:
- a non-magnetic support; and
a magnetic layer which is provided on the support and contains ferromagnetic powder and a binder,wherein the ferromagnetic powder is ferromagnetic hexagonal ferrite powder,the magnetic layer contains an abrasive,an intensity ratio (Int (110)/Int (114)) of a peak intensity Int (110) of a diffraction peak of (110) plane of a crystal structure of the hexagonal ferrite, determined by performing X-ray diffraction analysis on the magnetic layer by using an In-Plane method, to a peak intensity Int (114) of a diffraction peak of (114) plane of the crystal structure is equal to or higher than 0.5 and equal to or lower than 4.0,a squareness ratio of the magnetic recording medium in a vertical direction is equal to or higher than 0.65 and equal to or lower than 1.00, anda logarithmic decrement obtained by performing a pendulum viscoelasticity test on a surface of the magnetic layer is equal to or lower than 0.050.
1 Assignment
0 Petitions
Accused Products
Abstract
The magnetic recording medium includes a non-magnetic support and a magnetic layer which contains ferromagnetic powder and a binder, in which the ferromagnetic powder is ferromagnetic hexagonal ferrite powder, the magnetic layer contains an abrasive, Int (110)/Int (114) of a crystal structure of the hexagonal ferrite, determined by performing X-ray diffraction analysis on the magnetic layer by using an In-Plane method, to a peak intensity of a diffraction peak of (114) plane of the crystal structure is equal to or higher than 0.5 and equal to or lower than 4.0, a squareness ratio of the magnetic recording medium in a vertical direction is equal to or higher than 0.65 and equal to or lower than 1.00, and a logarithmic decrement obtained by performing a pendulum viscoelasticity test on a surface of the magnetic layer is equal to or lower than 0.050.
142 Citations
7 Claims
-
1. A magnetic recording medium comprising:
-
a non-magnetic support; and a magnetic layer which is provided on the support and contains ferromagnetic powder and a binder, wherein the ferromagnetic powder is ferromagnetic hexagonal ferrite powder, the magnetic layer contains an abrasive, an intensity ratio (Int (110)/Int (114)) of a peak intensity Int (110) of a diffraction peak of (110) plane of a crystal structure of the hexagonal ferrite, determined by performing X-ray diffraction analysis on the magnetic layer by using an In-Plane method, to a peak intensity Int (114) of a diffraction peak of (114) plane of the crystal structure is equal to or higher than 0.5 and equal to or lower than 4.0, a squareness ratio of the magnetic recording medium in a vertical direction is equal to or higher than 0.65 and equal to or lower than 1.00, and a logarithmic decrement obtained by performing a pendulum viscoelasticity test on a surface of the magnetic layer is equal to or lower than 0.050. - View Dependent Claims (2, 3, 4, 5, 6, 7)
-