Black coating of high thermal emissivity and process for applying the same

  • US 2,891,879 A
  • Filed: 07/26/1957
  • Issued: 06/23/1959
  • Est. Priority Date: 07/26/1957
  • Status: Expired due to Term
First Claim
Patent Images

1. THE METHOD OF MAKING A HEAT-DISSIPATING, LOW REFLECTIVITY, ADHERENT BLACK COATING, SAID METHOD INCLUDING THE STEPS OF (1) MIXING (A) ONE PART BY WEIGHT OF FINELY DIVIDED ALUMINUM, AND (B) FROM 0.35 TO 20 PARTS BY WEIGHT OF AN ORGANOPOLYSILOXANE RESIN, (2) APPLYING SAID MIXTURE TO A BASE MEMBER, AND (3) HEATING SAID BASE MEMBER AND SAID MIXTURE IN A NONOXIDIZING ATMOSPHERE TO A TEMPERATURE BETWEEN 660*C. AND 1500*C.