Process of manufacturing authenticatable paper products
First Claim
Patent Images
1. The process of manufacturing and testing authenticatable paper comprising:
- (a) treating a slurry of papermaking fibers selected from the group consisting of bleached chemical pulp and high yield lignin containing mechanical pulp with from 50-200 lbs/ton of a water soluble fluorescent whitening agent so as to cause said fluorescent whitening agent to become attached to said fibers;
(b) mixing the treated fibers of step (a) with a bleached chemical papermaking furnish to achieve a concentration of treated fibers in the furnish of about 0.1-4.0 lbs/ton of the furnish;
(c) producing a paper product from the papermaking furnish of step (b); and
,(d) exposing the paper product of step (c) to long wave ultraviolet illumination to detect the presence of the individual treated fibers in the paper product wherein the individual treated fibers fluoresce blue.
10 Assignments
0 Petitions
Accused Products
Abstract
An authenticatable paper product is prepared by adding to a papermaking furnish fibers treated with from about 50-200 lb/ton of a fluorescent whitening agent (FWA). The paper made from the papermaking furnish will include fluorescent cellulosic fibers in an amount ranging from between 0.1-4.0 lb/ton to achieve FWA concentrations within the range of 1-20 ppm.
99 Citations
6 Claims
-
1. The process of manufacturing and testing authenticatable paper comprising:
-
(a) treating a slurry of papermaking fibers selected from the group consisting of bleached chemical pulp and high yield lignin containing mechanical pulp with from 50-200 lbs/ton of a water soluble fluorescent whitening agent so as to cause said fluorescent whitening agent to become attached to said fibers; (b) mixing the treated fibers of step (a) with a bleached chemical papermaking furnish to achieve a concentration of treated fibers in the furnish of about 0.1-4.0 lbs/ton of the furnish; (c) producing a paper product from the papermaking furnish of step (b); and
,(d) exposing the paper product of step (c) to long wave ultraviolet illumination to detect the presence of the individual treated fibers in the paper product wherein the individual treated fibers fluoresce blue. - View Dependent Claims (2, 3)
-
- 4. An authenticatable paper product prepared from a bleached chemical papermaking furnish wherein from about 0.1-14.0 lbs/ton of the furnish consists of papermaking fibers treated with from 50-200 lbs/ton of a water soluble fluorescent whitening agent so as to cause said fluorescent whitening agent to become attached to said fibers and achieve a concentration of the fluorescent whitening agent in the paper product of less than about 20 ppm, wherein said individual treated fibers are detectable under long wave ultraviolet illumination.
Specification