Photovoltaic module package
First Claim
Patent Images
1. A glass comprising, in mol %:
- 70-77 SiO2 4.5-10.5 Al2O3 >
0-5 B2O3 3-5 MgO>
0-5 CaO0-5 SrO1.8-11.8 Na2O0-3 ZnO0-6 K2O3<
R′
O≦
12, and7≦
R2O≦
13,wherein R′
O=MgO+CaO+SrO+BaO, R2O=Na2O+K2O, the glass has a Na release greater than 10 ppm in a buffered aqueous release test, a total Na+K release of less than 30 ppm in a buffered aqueous release test, a Tmargin=Tbreakdown−
T35kp>
10°
C., and a strain point greater than 565°
C.
1 Assignment
0 Petitions
Accused Products
Abstract
Fusion-formable sodium-containing aluminosilicate and boroaluminosilicate glasses are described. The glasses are particularly useful for controlled release of sodium—useful in semiconductor applications, such as thin film photovoltaics where the sodium required to optimize cell efficiency is to be derived from the substrate glass.
-
Citations
7 Claims
-
1. A glass comprising, in mol %:
-
70-77 SiO2 4.5-10.5 Al2O3 >
0-5 B2O33-5 MgO >
0-5 CaO0-5 SrO 1.8-11.8 Na2O 0-3 ZnO 0-6 K2O 3<
R′
O≦
12, and7≦
R2O≦
13,wherein R′
O=MgO+CaO+SrO+BaO, R2O=Na2O+K2O, the glass has a Na release greater than 10 ppm in a buffered aqueous release test, a total Na+K release of less than 30 ppm in a buffered aqueous release test, a Tmargin=Tbreakdown−
T35kp>
10°
C., and a strain point greater than 565°
C.- View Dependent Claims (2, 3, 4, 5, 6, 7)
-
Specification