1. A process comprising the steps of:

  • a. applying at least one particulate material in the form of a loose powder; and

    b. separately applying a bonding agent over a portion of the at least one particulate material for selectively bonding the at least one particulate material;

    wherein a setting time is at least several times as long as an application time of a layer of the at least one particulate material;

    wherein the process is a process for layerwise construction of a three-dimensional component in a bed of the loose powderwherein the process includes a step of hardening a layer of the three-dimensional component after applying at least 20 subsequent layers.