Method for calendering pure copper foil

Method for calendering pure copper foil

CN
  • CN 101,209,457 A
  • Filed: 12/25/2006
  • Published: 07/02/2008
  • Est. Priority Date: 12/25/2006
  • Status: Active Application
First Claim
Patent Images

1. the method for a calendering pure copper foil may further comprise the steps:

  • A, with 0.08-0.12mm fine copper band annealing in process;

    B, fine copper band are cold rolling on cold-rolling mill, make Copper Foil,It is characterized in that;

    among the described step a, copper strips is positioned in the annealing furnace, and the annealing furnace temperature is set to 350-550 ℃

    , and annealing time 6-8 hour, the insulation of annealing back was taken out, and is cooled to room temperature.