1. be used to prepare the method for polyester polyol, wherein willAt least a carboxylic acid anhydride (A), glycol ether (B) withAt least a C 2-C 4Glycol (C) and at least a aliphatic C 5-C 12Dicarboxylic acid (D), Perhaps at least a C 5-C 10Glycol (E) and at least a C 4Dicarboxylic acid (F) mixes, Be characterised in that component (B) and (A) mol ratio are 1.5:

  • 1 –

    1.1;

    1, and based on the weight of all components of mixture, component (A) and weight quota (B) are 66 –

    , 95 weight %.