1. the brilliant glass-painting preparation method of boring, the described brilliant glass-painting that bores comprises layer glass plate, is provided with a brilliant drilling pattern layer between layer glass plate, brilliant drilling pattern layer and layer glass plate are adhesively fixed, and it is characterized in that:

  • described method comprises the steps;

    (1) be divided into multiple pattern units taking complete brilliant drilling pattern layer as pattern unit, or by brilliant drilling pattern layer, each pattern unit comprises at least one brilliant boring;

    (2) on the first glass plate, the crystalline substance of sticky the first pattern unit bores;

    (2-1) get the brilliant flat punch die boring of the first kind in the first pattern unit, flat punch die be surface be provided with corresponding pattern unit in the brilliant mould that bores the flat corresponding brilliant drill jig of one end shape chamber of corresponding kind, the crystalline substance of all inserting a corresponding kind in all brilliant drill jigs chamber bores, and the brilliant tip boring upwards;

    (2-2) get taper hole mould, described taper hole die edge has the half-cone die cavity being obtained by the center cutting of brilliant drill jig chamber, the most advanced and sophisticated half of shape that the crystalline substance of half-cone die cavity and adjacent patterns cell edges bores is corresponding, taper hole mould be surface be provided with corresponding pattern unit on the mould in all brilliant corresponding brilliant drill jig of pointed shape chambeies of boring, the die cavity place of taper hole mould is faced down, alignment taper hole mould peace punch die, two moulds are compressed and overturn, take off flat punch die, crystalline substance is bored and inserted in taper hole mould;

    (2-3) on the first glass plate, be coated with upper glue layer, glue-line the first glass plate is pressed on taper hole mould down, after curable adhesive layer, take off taper hole mould, the flat one end of brilliant brill adheres on the first glass plate, forms the first kind pattern of the first pattern unit on the first glass plate;

    (2-4) according to step (2-1), (2-2) and (2-3) make the brilliant pattern boring of other kind in the first pattern unit;

    On the first glass plate, complete and make the first pattern unit;

    (3) bore according to the crystalline substance of step (2) sticky other pattern unit on the first glass plate;

    (4) the first glass plate is alignd with the second glass plate, brilliant boring between the first glass plate and the second glass plate filled adhesive curing between two glass plates.