1. a method that improves molecular sieve catalyst intensity, comprises the following steps successively:

  • 1) acid solution that is 0.5~

    4 by pH value is processed molded molecular sieve catalyst, and treatment temperature is 100~

    300 ℃

    , and the processing time is 1~

    200 hour, and the weight ratio of acid solution and molded molecular sieve catalyst is 3~

    100;

    1;

    2) to the molded molecular sieve catalyst after processing be dried, after roasting finished catalyst.