1. The preparation method'"'"'s of the profiling polar region floating ice that a kind of technique ice-snow decorative landscape uses claim is:

  • described in description, preparation method comprises the steps;

    1. described in, preparation method comprises the steps;

    1), color deep ocean surface, polar region, choppy scene are drawn or air brushing on spray painting cloth, more stand-by on the position that its solidating is specified in view place;

    2), by special engraving benzene plate material by design specification size in advance, with pulling the external force that presses work, to make it fragment into nature cleavage block stand-by;

    3), the paraffin after melting is melted to liquid hairbrush and is coated in equably on nature benzene plate break, preferably benzene plate break is put in wax liquid into rapid soaking once;

    4), the profiling polar region floe being substantially shaped is selected to the floating rule of the natural floating ice that area less, following area in top is larger, be coated with behind the fast bottom of its profiling polar ice with pure concentration milky white adhesive again, its compacting be cemented on the spray painting cloth that is sprayed with ocean surface, polar region pattern;

    5), the matrix of the profiling polar region floating ice having prepared is covered to upper thick accumulated snow, it is that the preparation method of ZL200810127195.0 accumulated snow completes that the method and technology that covers accumulated snow can be selected the patent No., and technique profiling polar region floating ice accused and prepared.