1. adopt a Method of printing for the 3D printer of nylon material, it is characterized in that, comprise step:

  • Nylon material is dried 2-10 hour in 50-100 DEG C;

    Regulate the heater of 3D printer to level;

    The printer main body for printed product of sealing 3D printer, opens heater and temperature is set 60 DEG C-150 DEG C, and preheating 10-120 minute, make to be located at temperature in the coaming plate shell outside 3D printer main body and rise to 35-110 DEG C;

    Nylon material after drying is introduced in the fuse mechanism of printer main body;

    Printing adhesive base plate being smeared preset thickness;

    During the work of 3D printer main body, heater temperature maintains 60-150 DEG C, arranges the print speed of 3D printer main body at 20-200mm/s.