1. the shaping solid mould of toughened glass, is characterized in that:

  • it adopts following step to make;

    1. band radian toughened glass internal surface spread at least one deck glass wool cloth as convex glass silk cloth (1);

    2. a circle reinforcing bar (2) is added at the internal surface of convex glass silk cloth after having spread;

    3. repave on reinforcing bar after adding reinforcing bar at least one deck glass wool cloth as concave glass silk cloth (3);

    4. after coating style keeping liquid on the internal surface of concave glass silk cloth, at room temperature dry 25-35min both obtained again.