The method that two kinds of microporous crystals coordinate conversion to prepare SAPO 34 molecular sieve

The method that two kinds of microporous crystals coordinate conversion to prepare SAPO 34 molecular sieve

  • CN 106,082,266 A
  • Filed: 05/31/2016
  • Published: 11/09/2016
  • Est. Priority Date: 05/31/2016
  • Status: Active Grant
First Claim
Patent Images

1. the method that two kinds of microporous crystals coordinate conversion to prepare SAPO-34 molecular sieve, it is characterised in that through following step:

  • by crystalline substanceBody micropore aluminium phosphite NKX-2, A type molecular sieve, organic formwork agent and water mix homogeneously, temperature is 15~

    35 DEG C, then shouldMixture hydrothermal crystallizing 3~

    6 days under 165-200 DEG C and self-generated pressure, then cool down, wash, separate, room temperature is dried and producedThing, reaction mass has following mole of composition;

    Al2O3

    P2O3

    SiO2

    R∶

    H2O=1.0;

    1.0;

    0.67;

    (2.0~

    3.0);

    (35~

    100).