1. , a kind of heat preservation energy-saving decorative block and manufacture method, its core is to select for use modified polyamine fat to make thermal conductivity≤

  • 0.028w/ (m.k), what its surface daub on a wall layer was selected for use is benzene emulsion, pure-acrylic emulsion, organosilicon crylic acid latex, unsaturated polyester is that base-material is made, it is characterized in that;

    the batching of core is;

    comprise polyethers 100 in the A material, catalyzer 2.0-5.0;

    organotin 0.5-1.5, triethylamine, trolamine 1.0-3.0, suds-stabilizing agent;

    silicone oil 1.0-5.0, whipping agent;

    water 2.0-5.0, properties-correcting agent;

    season is defended tetrol, glycerine, Viscotrol C, optional wherein any consumption is 5-15;

    Comprise carbimide 100-130 in the B material;

    Above A expects more synthetic than mixing by weight, with the demoulding behind A material and the B material injection foaming machine mechanically mixing injection mould reflection curing molding;

    The surface daub on a wall layer formula;

    the base-material of selecting for use is;

    benzene emulsion, pure-acrylic emulsion, organosilicon crylic acid latex, unsaturated polyester are wherein chosen any one kind of them, quantity is 100, filler;

    stone flour, talcum powder, ground silica, choose any one kind of them or two kinds of total consumptions are 350-400, pigment;

    the needs color according to product is selected different pigment for use, total consumption is 5-10, auxiliary agent;

    thinner, film former, solidifying agent, dispersion agent, defoamer, flow agent, mould inhibitor, above each material is made ornament layer coating then than mechanically mixing by weight;

    Various auxiliary agents are decided according to feelings, and total consumption is 3-10, ornament layer coating is placed on the core surface with scraper it is wipeed off.