1. one kind is the colouring method of the polar fleece product of raw material with the wool, it is characterized in that comprising pre-treatment and staining procedure, in pre-treatment step, with 0.5-1.0 grams per liter soda ash the pH value is adjusted into 7.5-8.5, and temperature is 50-60 ℃

  • , and temperature retention time is 8-15 minute;

    In staining procedure, the pH of adjustment dye bath earlier value is 6-7, adds ACID DYES and auxiliary agent then;

    35-45 ℃

    of operation 5-15 minute, heat up with 0.5-1.5 ℃

    /minute speed, insulation is 20-35 minute in the time of 50-65 ℃

    ;

    Be warming up to 90-100 ℃

    more at the same rate;

    Be incubated 30-45 minute, be cooled to 40-60 ℃

    at last at the same rate, after the discharge opeing with hot water and cold water washing.