1. Make ferromagnetic oxide powders such as dispersant and Ba, Sr with paraffin and mix, magnetic 90~

  • 70 (wt%), paraffin 10~

    30 (wt%) adds a small amount of surfactant in addition, is shaped with the hot pressing injector that is added with magnetic field.Forming temperature 60~

    100 (℃

    ), mold temperature 25~

    50 (℃

    ), shaping pressure is several~

    tens (kgf/cm 2), profiled magnetic field 4000~

    7000 (oe) or use pulsed magnetic field, the ferritic manufacture method of the high orientation of the back dewaxing and sintering that is shaped.