METHOD FOR FILLING AT LEAST ONE CAVITY OF A MULTI-LAYER COMPONENT WITH A FILLING MATERIAL, AND MULTI-LAYER COMPONENT
First Claim
1. A method for filling at least one cavity (5a, 5b) of a multi-layer component (1) with filling material (9), comprising the following steps:
- A) providing a main body (2) of the multi-layer component (1), the main body (2) having at least one cavity (5a, 5b),B) placing the main body (2) in a chamber (11),C) generating a first pressure, the first pressure being a negative pressure,D) arranging the filling material (9) on the main body (2).
2 Assignments
0 Petitions
Accused Products
Abstract
The invention relates to a method for filling at least one cavity (5a, 5b) of a multi-layer component (1) with filling material (9). In a first step, the method comprises providing a main body (2) of the multi-layer component (1), the main body (2) having at least one cavity (5a, 5b). In a subsequent step, the method comprises placing the main body (2) in a chamber (11) and then generating a first pressure, the first pressure being a negative pressure. Then, a filling material (9) is arranged on the main body (2). Furthermore, the invention relates to a multi-layer component (1). The multi-layer component (1) has a main body (2) with at least one cavity (5a, 5b), wherein the cavity (5a, 5b) is filled with a filling material (9) which has a viscosity of between 200 mPas and 2000 mPas.
4 Citations
15 Claims
-
1. A method for filling at least one cavity (5a, 5b) of a multi-layer component (1) with filling material (9), comprising the following steps:
-
A) providing a main body (2) of the multi-layer component (1), the main body (2) having at least one cavity (5a, 5b), B) placing the main body (2) in a chamber (11), C) generating a first pressure, the first pressure being a negative pressure, D) arranging the filling material (9) on the main body (2). - View Dependent Claims (2, 3, 4, 5, 6, 7, 8, 9, 10, 11, 12, 13)
-
- 14. A multi-layer component, having a main body (2) with at least one cavity (5a, 5b), wherein the cavity (5a, 5b) is filled with a filling material (9) which has a viscosity of between 200 mPas and 2000 mPas.
Specification